Alright folks here is my delima. I purchased what a guy claimed was lexan recently and I have made a few panels for a bodiless out of it and the darn stuff simply keeps cracking every time I lay it over on the rocks. Is it possible that paint dry's out lexan or I am guessing I might have been duped and did not get lexan.
That being said what thickness lexan would you guys recommend for a bodiless? Thanks.
RickM